Conversion roasting: The spodumene concentrate is manually sent from the concentrate silo via the bucket elevator to the concentrate silo, and then added to the tail of the lithium carbonate rotary kiln via the disc feeder and the screw feeder. The tail gas preheating section high temperature gas drying concentrate, the concentrate is crystallized and calcined at a temperature of about 1200 ° C in the calcination section, and is converted into β-type spodumene by α type (monoclinic system, density 3150 kg/m3). The tetragonal system has a density of 2400 kg/m3, that is, a baking material, and the conversion rate is about 98%. |